Changing Operating Conditions
The evolution of industrial energy systems is intensifying the problem. Hydrogen infrastructure, carbon capture, and deeper offshore reservoirs create operating conditions that expose weaknesses in conventional sealing strategies. Hydrogen is particularly demanding because it combines an exceptionally small molecular size with extreme operating conditions. This compounds the challenges posed by permeation, pressure cycling, and rapid gas decompression.
Rapid gas decompression (RGD), also known as explosive decompression (ED), is becoming a key sealing challenge in hydrogen and CO2 capture facilities. Under pressure, gas molecules can penetrate deep into sealing materials. If the trapped gas must escape quickly during decompression, the seal effectively fails from the inside out unless the material structure is designed to accommodate this expansion. Composite materials engineered for RGD resistance maintain their structural integrity during depressurization.
The combination of cryogenic temperatures, high operating pressures, and repeated pressure cycling also places significant demands on thermoplastic components in critical valve systems (Figure 2). Thermoplastic seats in hydrogen pressure relief systems are one example. Even slight creep can allow small hydrogen molecules to escape through the pressure relief valve. To address this, a Fortune 500 company replaced its existing valve seat materials with Arlon® 3000XT, a cross-linked PEEK-based polymer.
Sealing components made from Arlon® 3000XT have been designed and tested to remain leak-free even at pressures above 20,000 psi (approximately 1,400 bar). Field use and high-pressure, high-temperature (HPHT) testing have demonstrated that Arlon® 3000XT outperforms conventional materials such as filled PEEK, making it suitable for seals, O-rings, and backup rings in hydrogen facilities (Figure 3).
These challenges are not limited to the hydrogen sector. CO2 capture and storage facilities also present their own material selection challenges. Supercritical carbon dioxide can leach plasticizers from lower-grade elastomers, causing them to become brittle and prone to cracking. Operators of CCS facilities must therefore consider decompression resistance, permeation behavior, and chemical resistance together.